Mostrar registro simples

dc.contributor.advisorBrunatto, Silvio Francisco, 1967-pt_BR
dc.contributor.otherScheuer, Cristiano José, 1986-pt_BR
dc.contributor.otherBorges, Paulo Césarpt_BR
dc.contributor.otherUniversidade Federal do Paraná. Setor de Tecnologia. Programa de Pós-Graduação em Engenharia Mecânicapt_BR
dc.creatorSevero, Fabiane da Silvapt_BR
dc.date.accessioned2024-01-31T21:51:11Z
dc.date.available2024-01-31T21:51:11Z
dc.date.issued2023pt_BR
dc.identifier.urihttps://hdl.handle.net/1884/86319
dc.descriptionOrientador: Prof. Dr. Sílvio Francisco Brunattopt_BR
dc.descriptionCoorientadores: Prof. Dr. Cristiano José Scheuer, Prof. Dr. Paulo César Borgespt_BR
dc.descriptionTese (doutorado) - Universidade Federal do Paraná, Setor de Tecnologia, Programa de Pós-Graduação em Engenharia Mecânica. Defesa : Curitiba,16/06/2023pt_BR
dc.descriptionInclui referênciaspt_BR
dc.descriptionÁrea de concentração: Manufaturapt_BR
dc.description.abstractResumo: O comportamento à erosão por cavitação do aço inoxidável martensítico tipo AISI 420 foi avaliado em solução 3,5% NaCl e em água destilada. As condições de estudo foram: aço cementado por plasma às temperaturas de 425, 450 e 475 ºC (após têmpera à 1050ºC) e aço temperado e revenido (têmpera a 1050ºC e revenimento a 220ºC). Neste estudo, foi verificado que as características de superfície (susceptibilidade à corrosão, relações entre dureza e módulo de elasticidade, fases presentes e sua morfologia na microestrutura) do material cementado influenciam na interação entre os processos de deterioração (processo oriundo do fenômeno de corrosão e processo oriundo do fenômeno de cavitação). As imagens obtidas por MEV demonstram que a intensidade da contribuição de cada fenômeno no processo total de desgaste variou com as distintas condições de tratamento recebidas pelas amostras. O período de incubação do aço temperado e revenido não apresentou alteração ao se variar o meio de ensaio (4,5 h). Porém, um período de aceleração mais extenso foi observado, quando o teste foi realizado em solução 3,5% NaCl. As amostras tratadas a 425 ºC e 450 ºC apresentaram um período de incubação maior que o da amostra não cementada no ambiente salino (16 h e 8,5 h, respectivamente), enquanto as amostras cementadas a 475 °C não apresentaram período de incubação.pt_BR
dc.description.abstractAbstract: The cavitation erosion behavior of the AISI 420-type martensitic stainless steel was evaluated in 3.5% NaCl and in distilled water. The studied conditions were plasma carburized steel at 425, 450 and 475 ºC temperatures (after quenching at 1050 ºC) and quenched and tempered steel (quenching at 1050 ºC and tempering at 220 ºC). In this study, it was verified that the surface characteristics (corrosion vulnerability, relationships between hardness and elasticity modulus, present phases and their morphology in the microstructure) of the carburized material influence the interaction between the deterioration processes (the process with origins in the corrosion phenomenon and the process with origins in the cavitation phenomenon). The images obtained by SEM demonstrate that the contribution intensity of each phenomenon to the total wear process varied with the different treatment conditions performed on the samples. The incubation period of the quenched and tempered steel did not change when the test medium was varied (4.5 h). However, a more extensive acceleration period was observed when the test was carried out in a 3.5% NaCl solution. The samples treated at 425 ºC and 450 ºC presented longer incubation periods than the untreated sample in the saline environment (16 h and 8.5 h, respectively), while the samples carburized at 475 °C did not present an incubation period.pt_BR
dc.format.extent1 recurso online : PDF.pt_BR
dc.format.mimetypeapplication/pdfpt_BR
dc.languagePortuguêspt_BR
dc.subjectProcesso de endurecimento superficialpt_BR
dc.subjectAço inoxidávelpt_BR
dc.subjectCavitaçãopt_BR
dc.subjectMateriais - Erosãopt_BR
dc.subjectEngenharia Mecânicapt_BR
dc.titleEstudo da resistência à cavitação em meio salino do aço AISI 420 cementado por plasma em condição de paraequilíbriopt_BR